Eric Jacobs:...
> I have Scotch 201 (acetate base) and Scotch 206 (polyester base, > back coated) in two dozen alternating segments. The Scotch 206 > is very sticky.
But is it really sticky shed?
I have over 500 reels of Scotch 207, LP version of 206, and all reels play as new with almost zero shedding of any sort.
BTW, I donĀ“t deny what you have seen, Eric, I just wonder if it is truly sticky shed?