631 is still good tape. I don't think anyone has reported problems with it. Definitely okay as leader for that purpose.

dl

Peoples, Curtis wrote:
We want to use it for head and tail leader only, not as separators.

-----Original Message-----
From: Association for Recorded Sound Discussion List
[mailto:ARSCLIST@xxxxxxx] On Behalf Of David Lennick
Sent: Wednesday, June 04, 2008 10:38 AM
To: ARSCLIST@xxxxxxxxxxxxxxxx
Subject: Re: [ARSCLIST] Ampex 631

Head and tail leader, or within the reel as separators? If that's the
purpose, it may not be visible in the pack, even with black oxide tape and
definitely not with brown oxide (499 etc).


CBC Edmonton never had leader tape around the place so the news and
current affairs department would just take 176 and splice it in BACKWARDS (oxide
out). Worked fine as leader, then somebody'd re-use the tape and wonder why
there were blank sections in the recording. And CBC Vancouver was using green
leader, which also wasn't visible in the pack.


dl

Peoples, Curtis wrote:


I have a couple of cases of Ampex 631 pro audio tape that is not going
to be used for recording purposes. Is there any reason why I cannot
use
it as leader tape? So far, I have not found 631 on any lists of tapes
with problems, such as sticky shed.



Curtis Peoples

Archivist

PO Box 41041
Texas Tech University
Southwest Collection/Special Collections Library
Lubbock, Texas 79409-1041
curtis.peoples@xxxxxxx
Phone: 806-742-3749 ext 265
Fax: 806-742-0496
www.swco.ttu.edu








[Subject index] [Index for current month] [Table of Contents]