Hi
I have just received 2 reels of 1/4inch tape recorded in 1968.
To the best of my knowledge this is the first time they have been played
since then.
They have been stored Tail Out
All the titles have been leadered with plain white plastic leader
The Tape has never been baked
When I spooled the first reel back to the start, to play, I found that
on 3 of the titles the oxide had adhered to the leader, having been
stripped off the tape backing. Thus rendering the first 3 or 4 seconds
unuseable.
This is obviously unrecoverable
When I came to the second side, I spooled up to the leader and the moved
the tape slowly by hand, the oxide is still sticking to the leader.
I have no idea what make the tape is, as it is not Emitape, but in an
EmiTape box
Has anyone met this, and how did you attempt to deal with it
Any help would be appreciated
Thanks
-pm
- --------------------------------------------------------------------
Music from EMI
This e-mail including any attachments is confidential and may be legally privileged. If you have received it in error please advise the sender immediately by return email and then delete it from your system. The unauthorised use, distribution, copying or alteration of this email is strictly forbidden. If you need assistance please contact us on +44 20 7795 7000.
This email is from a unit or subsidiary of EMI Group Limited.
Registered Office: 27 Wrights Lane, London W8 5SW
Registered in England No 229231.
- --------------------------------------------------------------------