At 02:42 PM 2007-12-04, Mew, Peter wrote:

All the titles have been leadered with plain white plastic leader
The Tape has never been baked
When I spooled the first reel back to the start, to play, I found that
on 3 of the titles the oxide had adhered to the leader, having been
stripped off the tape backing. Thus rendering the first 3 or 4 seconds
unuseable.

Did I say I hated plastic leader? ? ? ? ? I've never seen paper do this, despite its theoretical limitations. Sorry.


As to the problem, I've written Mr. Mew off-list, but there is not much definitive to say that's worth repeating to everyone until there is a repeatable success.

The goal would be to break the undesired bonds (the one from oxide to underlying leader) without breaking the desired bonds (oxide to original basefilm). It's akin to peeling sticky labels off things.

Cheers,

Richard

Richard L. Hess email: richard@xxxxxxxxxxxxxxx
Aurora, Ontario, Canada (905) 713 6733 1-877-TAPE-FIX
Detailed contact information: http://www.richardhess.com/tape/contact.htm
Quality tape transfers -- even from hard-to-play tapes.



[Subject index] [Index for current month] [Table of Contents]