> Would a simple
> cassette to wav to CDR work?

Yes

 Are there other steps that anyone would
> recommend to bring back or bring out what's on the tape?

Properly EQing each tape and checking the alignment of playback B4
digitizing. With cassettes, that have little heads and slow tape speeds,
alignment from machine to machine can be an issue.


-