[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: [ARSCLIST] Failed Cassette surgery
I can usually get these to work unless the tape itself is seriously
deteriorating. It takes about a half hour or so to fix.
Steve
-----Original Message-----
From: Association for Recorded Sound Discussion List
[mailto:ARSCLIST@xxxxxxx] On Behalf Of Peter Hirsch
Sent: Thursday, February 19, 2009 12:41 PM
To: ARSCLIST@xxxxxxxxxxxx
Subject: [ARSCLIST] Failed Cassette surgery
I have an audio cassette that had seized up and wouldn't play which I
rehoused
in a new shell. Apparently the shell wasn't the problem and my efforts
actually made matters considerably worse. Now I have a badly packed tape
that
has also torn off the leader. Rather than further mangle it, I give up and
would like to know who out there has the facilities to salvage this tape (or
at least attempt to). It's content is mostly unique archival material from
my
own collection of off-the-air and live performances from other sources and I
really do not want to give up on this one.
Thanks,
Peter Hirsch
punto@xxxxxxxx
(212) 569-8716 - home
(212) 714-8570 work (NYPL)
No virus found in this incoming message.
Checked by AVG - www.avg.com
Version: 8.0.237 / Virus Database: 270.11.0/1959 - Release Date: 02/18/09
20:55:00