At 12:46 PM 2007-01-10, Ed Falk wrote:
John Bondurant wrote:
Does anyone know of a reliable vendor for 1/4" paper leader tape? I
have had two vendors tell me they are out of stock and it looks
like (in their opinion) that this product has become obsolete.
IMHO, "reliable" and "paper leader tape" don't go in the same
sentence. I've had nothing but misery with old tapes that were
spliced with paper leader tape. Something in the paper reacts with
the splicing tape and the glue fails in about 20 years. I have not
had this problem with plastic leader tape.
In other words, yes, the product is obsolete.
On the other hand, I've had several instances of oxide laminating to
3M plastic leader tape and ripping off the backing. "In the day"
paper was preferred, though I never understood why. Now I do.
I have an adequate but not excessive stock of it for my use. Watch
ePay--it might show up again.
Cheers,
Richard
Richard L. Hess email: richard@xxxxxxxxxxxxxxx
Aurora, Ontario, Canada (905) 713 6733 1-877-TAPE-FIX
Detailed contact information: http://www.richardhess.com/tape/contact.htm
Quality tape transfers -- even from hard-to-play tapes.