--- David Lennick <dlennick@xxxxxxxxxxxx> wrote:

> Actually if anyone has an answer
> to this or to the related problem of musty record jackets and
> labels (a problem I'm facing with
> records I've been buying from an estate, where there was a flooded
> basement), let us know.

Book conservators usually place them in a vacuum chamber and
draw the moisture out through evaporation.  If you heat the
paper you will probably both warp it and make it brittle.
A good way to preserve the book before the vacuum treatment 
is to freeze it.  Maybe you could have it freeze-dried by
a firm that processes freeze dried food?


David Breneman         david_breneman@xxxxxxxxx