[Table of Contents]


[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]

Re: [ARSCLIST] To keep the tapes or not



Too true, all of it. I was just thinking of how to recycle it, not to be a good source of tape... Never mind!

Lou Judson • Intuitive Audio
415-883-2689

On Dec 10, 2005, at 9:30 AM, Tom Fine wrote:

Who would want bulk-erased acetate vinegar-ish tape stock?

Then again, eBay sharks regularly unload sticky-shed era Ampex tape on
suckers.

Anyone who is serious about tape recording should start with new stock or at
least NOS tape that they have kept under proper conditions and know for sure
is not prone to sticky-shed.


-- Tom Fine