In a message dated 10/6/2005 3:03:09 PM Eastern Daylight Time, 
ArcLists@xxxxxxxxxxxxxxx writes:
I placed the tape in an open container inside a sealed container. The 
sealed container had about an inch of water in the bottom. The tape 
was up on spacers in the open container. This was room temperature.
***************

Some early Kodak 16 mm film cans had a built-in perforated chamber containing 
blotting paper for just this purpose. Of course it is not recommended that 
acetate material be stored this way.