The recommendation is to use a water-based permanent marker and to write
only on the hub.  The Dixon RediSharp Plus is one marker being recommended.
Manufacturers of CD-Rs also supply markers that they say are suitable but
find out if they are water-based.  Writing on the non-hub area introduces
an element of risk.  Will there be penetration through the top layers and
eventual corrosion of the metal layer?  It is not known which markers would
do this and how resistant top layers of different CDs are to such an
effect.  Therefore, writing on the hub removes this risk.

Joe Iraci
Conservation Scientist
Canadian Conservation Institute


                                                                                                                                          
                      Anthony Bozzanca                                                                                                    
                      <abozzanca@xxxxxxxxx        To:       ARSCLIST@xxxxxxxxxxxx                                                         
                      SUNYSB.EDU>                 cc:                                                                                     
                      Sent by: Association        Subject:  Re: [ARSCLIST] CD-R hub labels...                                             
                      for Recorded Sound                                                                                                  
                      Discussion List                                                                                                     
                      <ARSCLIST@xxxxxxx>                                                                                                  
                                                                                                                                          
                                                                                                                                          
                      07/05/2003 05:33 PM                                                                                                 
                      Please respond to                                                                                                   
                      Association for                                                                                                     
                      Recorded Sound                                                                                                      
                      Discussion List                                                                                                     
                                                                                                                                          
                                                                                                                                          





That's what I heard about putting labels in the disc as well. What's the
general consensus about using a fine point sharpie marker to write on the
CD's to label them?

Anthony Bozzanca
Recording Engineer
Music Library
Stony Brook University
www.sunysb.edu




                                                                           
       Joe_Iraci@xxxxxxxxx                                                 
       Sent by: Association for                   To:                      
       Recorded Sound Discussion          ARSCLIST@xxxxxxxxxxxx            
       List <ARSCLIST@xxxxxxx>                    cc:                      
                                                  Subject:        Re:      
       05/07/2003 03:09 PM                [ARSCLIST] CD-R hub labels...    
       Please respond to                                                   
       Association for Recorded                                            
       Sound Discussion List                                               
                                                                           
                                                                           




By putting the adhesive label on the hub you are less likely to experience
balance and warping problems.  Also, delamination of the top layers is
unlikely as well unless you overlap onto the lacquered area of the disc.
However, as you know adhesive labels are not recommended for maximum
longevity.   Over time, aging of the label leading to oozing of adhesive,
partial lifting of the label, and possible chemical reactions between the
label components and disc can cause problems.  Therefore, for short-term
use this type of label is less problematic than labels that cover the whole
disc, but I would stay away from them if you want to maximize your disc
lifetime.

Joe Iraci
Conservation Scientist
Canadian Conservation Institute



                     andy kolovos
                     <akolovos@VERMONTFOLKLIFE        To:
ARSCLIST@xxxxxxxxxxxx
                     CENTER.ORG>                      cc:
                     Sent by: Association for         Subject:  [ARSCLIST]
CD-R hub labels...
                     Recorded Sound Discussion
                     List <ARSCLIST@xxxxxxx>


                     07/05/2003 02:11 PM
                     Please respond to
                     Association for Recorded
                     Sound Discussion List






ARSC-Folks,

Anyone have an experience using those tiny labels that adhere to the
plastic inner hub of CD-Rs?  Writing on the hubs--which is ok for in-house
stuff but still kind of a pain in the neck--is a real pain when creating
CD-R copies of materials to go out to researchers, and looks pretty bad
when making copies for people who have ordered recordings from the archive.
While I'm inclined just to buy a CD-Stomper sort of thing for labeling
copies of ordered materials, I'd rather legibly type info on to a hub label
for in-house use (as opposed to master) copies and copies made for
researchers who donate their materials to us.

The labels I'm talking about in particular are Gaylord item# DY-249CL.

http://www.gaylordmart.com/adblock.asp?abid=88&sid=0EBA8076E92A454381FBE8BF0

009B2&search_by=desc&search_for=cd%20label

Any thoughts?

Thanks,

Andy

*********************************
Andy Kolovos
Archivist/Folklorist
Vermont Folklife Center
P.O. Box 442
Middlebury, VT 05753
(802) 388-4964
akolovos@xxxxxxxxxxxxxxxxxxxxxxxxx
http://www.vermontfolklifecenter.org






[Subject index] [Index for current month] [Table of Contents]