Use cardboard cut to size (square), or a fraction
over. And use plenty of pieces on each side of the
records. 

The important point is to alternate the direction of
the cardboard. - | - | - | - 
That drastically increases the strength and reduces
the likelihood of bends. Tape with a moderate degree
of tightness, do not make it loose or overly tight.

I spent many years auctioning records and sent
thousands of records all over the world. 





=====
Dr. Cheryl Thurber email: cthurb@xxxxxxxxx
P.O. Box 9447, Baltimore, MD 21228-0447

New phone # 410-747-5557

__________________________________________________
Do you Yahoo!?
Yahoo! Mail Plus - Powerful. Affordable. Sign up now.
http://mailplus.yahoo.com
-
For subscription instructions, see the ARSC home page
http://www.arsc-audio.org/arsclist.html
Copyright of individual posting is owned by the author of the posting and
permission to re-transmit or publish a post must be secured
from the author of the post.


[Subject index] [Index for current month] [Table of Contents]