At 02:29 PM 3/11/2002 -0500, Monica Fazekas wrote:
Hello everyone,
To begin with, thank you for your responses and suggestions regarding
our problems with the vinyl sleeves.  For further clarification we are
not putting any labels of any type on the CDs.  These are commercial CDs
and what I mean by "label" is the side of the CD with the manufacturer's
printed information on it.  The sticking is generally happening on this
side (although I suppose in time it could stick to the other side as
well.

Sticking to the polycarbonate bottom layer is far less likely. The problem is with the inks and possibly with the acrylic lacquer under them on the printed surface.


Mike

mrichter@xxxxxxx
http://www.mrichter.com/


- For subscription instructions, see the ARSC home page http://www.arsc-audio.org/arsclist.html Copyright of individual posting is owned by the author of the posting and permission to re-transmit or publish a post must be secured from the author of the post.


[Subject index] [Index for current month] [Table of Contents]