combination tanned

A general term sometimes applied to a leather tanned by two or more tanning processes. Combination processes include CHROME TANNING followed by VEGETABLE TANNING , i.e., CHROME RETAN ; vegetable tanning followed by chrome tanning, or SEMI-CHROME TANNAGE : tanning with formaldehyde followed by treatment with oil, orCOMBINATION OIL TANNAGE .