2. Watermarked office papers, permanent, for use in dissertations.

Badger Paper Mills, Inc.: Tanonka Premium #1 Watermarked Bond. "Marks of Distinction" Private Watermark. Call 800/826-0494.

Crane & Co., Inc.: Thesis. Call 413/684-2600.

Crown Vantage, Inc.: Graphika! 25% Cotton: Contains 20% PCW (post-consumer waste); 24# watermarked; laser and inkjet guaranteed. Retreeve Writing: Contains 20% PCW; 24# watermarked; laser and inkjet guaranteed. Brightwater Ultra Smooth and Riblaid: 99 Brightness; 24# acid-free and CaCO3 buffered; manufactured to laser and inkjet finish specifications; no watermark. Private watermarks are made to order for corporations, universities and other users. They can be used in any of Crown Vantage's market brands of writing grades, depending on the size of the order. Call 800/421-8289.

Fox River Paper Co.: Howard Permalife Bond and Ledger are both watermarked as Permalife. They are also both 25% cotton. Call 800/558-8327.

Eastern Fine Paper, Inc.: Atlantic Bond and Certificate Bond. Call 413/549-7635.

Esleeck Manufacturing Co., Inc.: Private watermarks can be made to order for use on papers manufactured for corporations or universities. CaCO3 buffered. Choice of cotton or wood fiber, Bright White or Off-White. Call 413/863-4326.

Neenah Paper: Old Council Tree® Writing, Atlas® Bond, Neenah® Laser Recycled, Classic Crest® Recycled Writing. Call 800/241-3405.