1. Here are two images from the textiles that were infested in the past from mould.
2. I would very much appreciate if anyone knows any articles or research on KIERLAON OLB KONZ as a detergent fro textiles (aprticularly wool I believe). Is the first time I have found some but since never used here I would like to know more on it before do some tests.
Many thanks
Konstantinos Chatziantoniou
Musuem of Islamic Art
Doha
Qatar
Date: Fri, 20 Feb 2009 10:08:18 -0500
From: BallardM@xxxxxx
Subject: Re: Mould infestation on excavated ancient costumes
To: TEXCONS@xxxxxxxxxxxxxxxxxx
Konstantinos: You have looked at the white spots under the microscope? Can you scrap a few off and see if they dissolve in water? Have a pH? What kind of a box? Where was the box stored? Send us a photo? Mary
Mary W. Ballard
Senior Textiles Conservator,
Museum Conservation Institute, Smithsonian Institution
4210 Silver Hill Road, Suitland MD 20746 U.S.A.
tel: 301-238-1210 fax: 301-238-3709
email ballardm@xxxxxx
From: Textile Conservators [mailto:TEXCONS@xxxxxxxxxxxxxxxxxx] On Behalf Of K Hatziantoniou
Sent: Friday, February 20, 2009 6:36 AM
To: TEXCONS@xxxxxxxxxxxxxxxxxx
Subject: Mould infestation on excavated ancient costumes
Importance: High
Dear all
I found extensive mould infestation (white spots covering the whole robes including the linings) on costumes whihc are folded in layers and placed for years in the same box. I have nevere seen these costumes before as this is the first time I opened the box for survey of the textiles. The alarming incident needs direct attention. Except from surface cleaning, can anyone suggest imediate measurements and if possible materials that could help on this? Storage conditions are stable but the collection has been moving around for several years. Since excavation it is known to me of any treatment for possible mould attack on these pieces from previous owners/conservators.
The costumes are all silk with metal threads.
Thank you for your time and help
Konstantinos Chatziantoniou