new textile for historic aeroplane
Dear all,
we are in the process of conservation a historic aeroplane and would like to cover it with a new textile. The aim is to let the aeroplane fly again. The new covering is to match the old one. Therefore, we are looking for a textile which is specifically made for this purpose. It has to fulfil the following demands (German Standarts DK 677.064:629.73 of 1968):
- cotton yarn 100 dtex x2
- plain weave, wrap desity 33 +/- 2 threads per cm; weft-density 33 +/- 2 threads per cm
- finishing: mercerisised, mould-inhabitant
- width: minimum 130 cm
- weight: 135 g/m2 +/- 5%
- maximum elongation per warp an weft 13% (at 850 kg)
- tensile strength per wrap and weft: 1300 kg/m
thanks very much for your information to find such a fabric! Julia
Dipl. - Rest. Julia Dummer
Museumslandschaft Hessen Kassel
Textil- und Lederrestaurierung
Postfach 410 420
D – 34 066 Kassel
Fon 0049 (0) 561 316 80 326
Fax 0049 (0) 561 316 80 333
j.dummer@xxxxxxxxxxxxxxxx
www.museum-kassel.de
--
GMX startet ShortView.de. Hier findest Du Leute mit Deinen Interessen!
Jetzt dabei sein: http://www.shortview.de/wasistshortview.php?mc=sv_ext_mf@gmx