Hello Julia - just the other day, on National Public Radio, I heard a
story about a reconstructed Wright Flyer that was built to commemorate
the first US military flight. The story as broadcast mentioned the
fabric, which was (as I understand it) made in the same way as the
original fabric. Here is a link to the NPR story:
http://www.npr.org/templates/story/story.php?storyId=94332520, and here
is a link to the organization that built it
http://www.wrightexperience.com/. Maybe they can help you find what you
need.
Cordially,
Mary Montgomery
Curator/Librarian
Museum of History & Industry, Seattle
-----Original Message-----
From: Julia Dummer [mailto:JuliaDummer@xxxxxx]
Sent: Tuesday, September 09, 2008 3:30 AM
To: TEXCONS@xxxxxxxxxxxxxxxxxx
Subject: new textile for historic aeroplane
Dear all,
we are in the process of conservation a historic aeroplane and would
like to cover it with a new textile. The aim is to let the aeroplane fly
again. The new covering is to match the old one. Therefore, we are
looking for a textile which is specifically made for this purpose. It
has to fulfil the following demands (German Standarts DK 677.064:629.73
of 1968):
- cotton yarn 100 dtex x2
- plain weave, wrap desity 33 +/- 2 threads per cm; weft-density
33 +/- 2 threads per cm
- finishing: mercerisised, mould-inhabitant
- width: minimum 130 cm
- weight: 135 g/m2 +/- 5%
- maximum elongation per warp an weft 13% (at 850 kg)
- tensile strength per wrap and weft: 1300 kg/m
thanks very much for your information to find such a fabric! Julia
Dipl. - Rest. Julia Dummer
Museumslandschaft Hessen Kassel
Textil- und Lederrestaurierung
Postfach 410 420
D - 34 066 Kassel
Fon 0049 (0) 561 316 80 326
Fax 0049 (0) 561 316 80 333
j.dummer@xxxxxxxxxxxxxxxx
www.museum-kassel.de
--
GMX startet ShortView.de. Hier findest Du Leute mit Deinen Interessen!
Jetzt dabei sein:
http://www.shortview.de/wasistshortview.php?mc=sv_ext_mf@gmx