Re: Cellulose/polyethylene terphthalate blends



Jamie

Without having cracked open a book or anything, I'd say 1941 is probably about right: PET was one of the fibers developed under the auspices of the Army/the Textile Research Institute in the ramp-up to the Second World War.

Best regards

Sarah

Sarah Lowengard
sarahl@xxxxxxxxx
New York City