Hello everyone,

   I was talking to our paper conservator today about the deacidification of
paper.  He was wondering if textile conservators use similar chemicals to
deacidify textiles.  They use Calcium Hydroxide or Magnesium Bicarbonate.  I had
never heard of using these chemicals with textiles.  Does anyone know if these,
or similar chemicals are ever used in the treatment of textiles?

Thanks,

Jennifer

Jennifer Hadley
Collections Care
Museum of Church History and Art
(801) 240-0297
hadleyj@xxxxxxxxxxxxx

----------------------------------------------------------------------
NOTICE: This email message is for the sole use of the intended recipient(s) and may contain confidential and privileged information. Any unauthorized review, use, disclosure or distribution is prohibited. If you are not the intended recipient, please contact the sender by reply email and destroy all copies of the original message.


[Subject index] [Index for current month] [Table of Contents] [Search]