Hi Carol,
Unfortunately I won't see the suit until right before
the installation. I won't be able to answer questions
before then.
Thanks, Nancy
--- Amann Conservation
<amann.conservation@xxxxxxxxxxx> wrote:
> Nancy,
> I have cleaned vinyl surfaces on several Pop-Art
> works of art. First my
> questions.
>
> Are these marks actually accretions (color on the
> surface) or loss of the
> surface layer? Is the vinyl matte or glossy?
> Is the vinyl thin or thick? Is it on a fabric
> support?
>
> Carol Kropnick
>
>
>
>
> -----Original Message-----
> From: owner-texcons@xxxxxxxxxxxx
> [mailto:owner-texcons@xxxxxxxxxxxx]On
> Behalf Of Nancy Love
> Sent: Wednesday, September 05, 2001 11:30 AM
> To: List Textiles
> Subject: cleaning vinyl
>
>
> Has anyone had experience removing scuff marks from
> vinyl? I have been asked to conserve, for
> exhibition,
> a 35 year year old yellow vinyl bathing suit. The
> suit has "scuff marks" (cause unknown). It has been
> suggested that I cover them over with pastels for
> the
> exhibition. Any ideas? I would appreciate
> suggestions as soon as possible.
>
> Thanks, Nancy Love
>
> __________________________________________________
> Do You Yahoo!?
> Get email alerts & NEW webcam video instant
> messaging with Yahoo! Messenger
> http://im.yahoo.com
>
__________________________________________________
Do You Yahoo!?
Get email alerts & NEW webcam video instant messaging with Yahoo! Messenger
http://im.yahoo.com