Re: [ARSCLIST] Lacquer disc storage conditions



Hopefully they are red label. It was their best lacquer disc and seem to
hold up better than their lower grades. At least by my experience.

B. Hodge 

-----Original Message-----
From: Association for Recorded Sound Discussion List
[mailto:ARSCLIST@xxxxxxx] On Behalf Of Jeffrey Martin
Sent: Wednesday, November 19, 2008 3:10 PM
To: ARSCLIST@xxxxxxxxxxxx
Subject: [ARSCLIST] Lacquer disc storage conditions

I'm trying to advise a colleague who has recently discovered some
1960s-era lacquer discs in her collection. (They're recorded on Audio
Devices Audiodiscs.)  What are the preferred conditions for storing
lacquer discs? She has access to cold storage (40 degrees F), cool
storage (55 degrees F) and obviously standard office HVAC storage.

Many thanks,

Jeff Martin
Chicago, IL