As you are aware, harmonic distortion is essentially integral multiples of the original frequency generated by nonlinearities in the signal chain. Some is generated at the acoustic source.

If you can reproduce more of these highs, then you'll hear them.

I tangentially touch on that in my Azimuth paper on my website http://richardhess.com/notes/2006/09/27/azimuth-hows-and-whys/
listen to the sample. You're doing the same thing but for spacing loss rather than azimuth loss.


Lately I've been using a spare tape deck controller card in my A810 so as not to mess up the calibrated one and readjusting tensions instead of using the thumb, but both work.

It is important to understand the cause of the spacing loss as you may be masking a transport problem -- or it just may be a damaged tape or a tape with poor slitting (i.e. damaged at birth).

Hope that helps.

Cheers,

Richard

At 11:58 AM 2007-04-04, Ganesh.Irelan@xxxxxxxx wrote:
Hello,

I sometimes apply manual pressure to old 1/4" tapes to increase tape to head contact during low speed playback. I have found this increases high frequency response. I have also found that it seems to increase harmonic distortion. Is the increase in distortion simply due to the additional high frequencies making it more audible? Is this an acceptable practice?

Richard L. Hess email: richard@xxxxxxxxxxxxxxx
Aurora, Ontario, Canada (905) 713 6733 1-877-TAPE-FIX
Detailed contact information: http://www.richardhess.com/tape/contact.htm
Quality tape transfers -- even from hard-to-play tapes.



[Subject index] [Index for current month] [Table of Contents]