Roger
Mike Richter <mrichter@xxxxxxx> wrote: D. Blake Werts wrote:
> This talk about the storage of CDs and LPs has me thinking... Are there any
> known issues with the storage of LPs in "plastic" bags? I have been using
> some of the nice re-sealable sleeves made available through Far West Record
> Supply (polypropylene?) and wondered if I will be causing damage in the long
> term with these?
>
> Any advice or experience that you can offer?
>
> Thanks Much!
> D. Blake Werts
It depends on the plastic.
We 'spoke' some time ago about plasticizer leaching out of some plastics
to clog the LP grooves. Even a light coating is lethal and it cannot be
removed without etching the vinyl. I've several old European EMIs that
died that unfortunate death.
Mike
--
mrichter@xxxxxxx
http://www.mrichter.com/
"If you're not on somebody's watchlist,you're not doing your job"
Dave Von Kleist
---------------------------------
The fish are biting.
Get more visitors on your site using Yahoo! Search Marketing.