Ya know, I was going to say that. Does that work with 78's??? I know it works with LPs because I've done it. Two thick pieces of plate glass and the oven on Warm (about 130 degrees in my mid-70's GE ovens). Electric ovens, of course!

-- Tom Fine

----- Original Message ----- From: "phillip holmes" <insuranceman@xxxxxxxxxx>
To: <ARSCLIST@xxxxxxxxxxxxxxxx>
Sent: Monday, October 23, 2006 6:30 PM
Subject: Re: [ARSCLIST] Record flattening



It's audiophool stuff. You can do the same thing with two pieces of glass and an oven.

Steven Smolian wrote:
In the current high-end catalog, Musicdirect, a record flattening machine is offered. It's at the bottom of p. 30 and called "Air Tight DT-01." Anyone have experience with it?

I can't find a manufacter on the net so can't ask him questions. How does it work on 78s is the big one.

Steve Smolian