Here is the best example I've seen that acetate tape's outgassing is
absorbed by the cardboard box. Presumably the brown areas of the box
are more acidic than the white areas, but I'm not really able to test that.
See:
http://richardhess.com/notes/2006/10/16/acetate-tape-buffered-by-cardboard-box/