[ARSCLIST] removing adhesive from CD case



what works great is a rubber cement "pick up" square. it's a square eraser that you can get at any hobby shop. rub it in one direction over the adhesive until it "balls" up and remove it. a regular rubber eraser can also work too if you can't find the rubber cement pick up.

less stinky than lighter fluid, goo gone and peanut butter.

hey, do people still want the disaster recovery handout for audio materials? i can send it to the list...