[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: [ARSCLIST] To bake or not to bake?
Thanks Tom. The former owner of the record company is wanting CDs of
his favorite music. THAT is on the 456 and the 226. The 206 and 207 are
old DBX safety copies from his personal archive. I just lumped them
together in my description...
Good question, if it were true...
<L>
Lou Judson • Intuitive Audio
415-883-2689
On Aug 14, 2006, at 2:55 PM, Tom Fine wrote:
Hi Lou:
Odds are VERY GOOD you WILL need to bake the Ampex 456 and Scotch 226
and VERY GOOD you WILL NOT have to bake the Scotch 206 and 207.
Curious -- what record label would master to Scotch 207? I was always
told never to use 1 mil tape for anything critical like a master.
-- Tom Fine