That was my experience with 468 as well... Although I thought it sounded
very good.
No free lunch....
-----Original Message-----
From: Association for Recorded Sound Discussion List
[mailto:ARSCLIST@xxxxxxx] On Behalf Of Karl Miller
Sent: Tuesday, June 20, 2006 9:53 AM
To: ARSCLIST@xxxxxxxxxxxxxxxx
Subject: Re: [ARSCLIST] Ampex 456 - tip of the iceberg...chemistry
On Sat, 17 Jun 2006, Steven Smolian wrote:
> Was Agfa 468 polyester?
I believe it was. My experience with it was miserable. I had never seen
tape ooze before. It was a mess within a few years.
Karl