[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: [ARSCLIST] Ampex 456 - tip of the iceberg...chemistry
Thanks very much for this considered postin, Richard. In the late 70s
we were using Shamrock 7" castoffs, and it seemed that some of it was
backcoated and some was not, as a manufacturing defect as the oxide
looked ad performed the same to our untrained ears. Would it be helpful
if I could ghet some samples like this? I'm not sure I can, and not
assurance that it was a similar batch if so, but it has me wondering...
Lou Judson • Intuitive Audio
415-883-2689
On Jun 16, 2006, at 5:05 PM, Richard L. Hess wrote:
We can create a hypothesis that back-coating in contact with binder
has a catalytic effect on the degradation of the binder.