[ARSCLIST] Squealing Scotch 996



I've just encountered a reel of Scotch 996 which is squealing. It does not
seem to exhibit any symptoms of sticky shed - no buildup on the heads, and I
was under the impression that 996 did not suffer from stick shed.

Any thoughts?

-- 
Konrad Strauss