[Table of Contents]


[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]

Re: [ARSCLIST] Ampex & Sticky Shed Syndrome



----- Original Message -----
From: "Rollin' Recording" <lou@xxxxxxxxxxxxxxxxxxx>
> I believe Shamrock Tape was b-stock from Ampex.  It was either "second
tier"
> i.e. had some quality issues, or perhaps just overstock.
Other posts suggested that Shamrock, like some other lower-priced brands,
was in some
cases reslit computer or other industrial tape.
Steven C. Barr


[Subject index] [Index for current month] [Table of Contents]