Re: [ARSCLIST] Ampex & Sticky Shed Syndrome



We have problems with 3M 808 & 809 purchased about 1990! 

We have a lot of earlier 3M 176 & 177 which doesn't exhibit any
symptoms.

Nigel Champion
Archive of Maori & Pacific Music
The University of Auckland
New Zealand


-----Original Message-----
From: Association for Recorded Sound Discussion List
[mailto:ARSCLIST@xxxxxxx] On Behalf Of Steve Green
Sent: Thursday, 16 December 2004 2:12 p.m.
To: ARSCLIST@xxxxxxxxxxxx
Subject: Re: [ARSCLIST] Ampex & Sticky Shed Syndrome

Thanks Richard,

Just curious, can you recall what the 3M tape stock was that first
raised the alarm? And about when was that?