"Richard L. Hess" wrote:

> 
> Anyone have any thoughts on a 1976 3M dictation cassette that's
> squeaking--not sticky shed? It is causing audible scrape flutter in the
> transfer.
> 

This is purely anecdotal and unscientific but I had an unbranded
cassette from around 1980 with similar symptoms. I tried playing it in
various machines over a few days with no joy. I would guess that there
was a problem with the tape lubricant.

In this case I left it for a few months and when I came back to it the
tape played perfectly without any problem. Maybe there was a difference
in humidity or temperature from its previous storage location but there
were no obvious or major changes.

Unfortunately I would guess that you don't have the time to wait a few
months.

Cheers.

James.
-
For subscription instructions, see the ARSC home page
http://www.arsc-audio.org/arsclist.html
Copyright of individual posting is owned by the author of the posting and
permission to re-transmit or publish a post must be secured
from the author of the post.


[Subject index] [Index for current month] [Table of Contents]