ANSI/PIMA standard IT9.25-1998 "Photography-Optical disk media-Storage" addresses the storage and housing of optical discs. This is also an ISO standard ISO/TC 42/SC N4335.

In section 6.1 it reads: "Container shall be resistant to impact, moisture and dust intrusion. Containers made of paper or cardboard shall not be used. Containers shall be designed in such a way that neither the disc data or label surface is in contact with the container when the container is stored in its proper vertical position. Containers shall not be able to be deformed, or mechanically compromised, in the defined storage conditions. The container lid shall be capable of being latched, attached, or locked to prevent accidental opening.

Plastics such as polystyrene, polypropylene, and polycarbonate are suitable for storage housing applications. Prolonged exposure to strong light, including fluorescent and incandescent lighting, causes yellowing of polystyrene plastics, sometimes accompanied by crazing. Polystyrene and polypropylene break down in sunlight or ultraviolet (UV). Foam rubber and plastics such as cellulosics, polyvinyl chloride (PVC), and highly plasticized materials shall be avoided."

This section basically describes a jewel box. It also specifically recommends against highly plasticized materials, of which vinyl is one. While tyvek is inert, it does touch the disc surface which is recommended against. I don't know the details of the standards making process and why this standard came out of PIMA (which makes photography and imaging standards), but if you read the whole standard they are essentially talking about audio CDs, CD-ROMs, Photo-CDs and other familiar optical discs.

Regards,
David Seubert, Curator
Performing Arts Collection
Davidson Library Special Collections
University of California
Santa Barbara, CA  93106
(805) 893-5444 Fax (805) 893-5749
mailto:seubert@xxxxxxxxxxxxxxxx
http://www.library.ucsb.edu/speccoll/pa/

-
For subscription instructions, see the ARSC home page
http://www.arsc-audio.org/arsclist.html
Copyright of individual posting is owned by the author of the posting and
permission to re-transmit or publish a post must be secured
from the author of the post.


[Subject index] [Index for current month] [Table of Contents]