Turkey morocco

1. Reputedly, a strong, durable leather produced in the 18th century in Turkey from goatskin, with the characteristic MOROCCO grain. 2. A term applied to a leather, frequently produced from calfskin, embossed with a hard grain or bold cross grain in imitation of a Turkey morocco. (129 , 264 )