cupriethylenediamine viscosity

The VISCOSITY (2) of a cellulosic solution or a paper pulp in cupriethylenediamine hydroxide under specified conditions, especially those of temperature, cellulose concentration, and solvent composition. It is used to determine the average molecular weight of the dissolved cellulose. (17 )