album paper

A type of cover paper used for photograph albums. It is manufactured in gray and black in basis weights of 50 to 80 pounds (20 X 26 – 500). A basic requirement of this paper is that it not cockle when wetted with adhesives, while another essential requirement is that it contain no impurities which might alter or damage the photographs. (17 , 324 )