[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: life span of vinyl fabric
Thank you very much! This will be great.
Jennifer
-----Original Message-----
From: Textile Conservators [mailto:TEXCONS@xxxxxxxxxxxxxxxxxx] On Behalf Of Joanne Hackett
Sent: Thursday, July 03, 2008 9:42 AM
To: TEXCONS@xxxxxxxxxxxxxxxxxx
Subject: Re: life span of vinyl fabric
Hello Jennifer,
Yvonne Shashoua did extensive research into PVC (vinyl) for her PhD. I
found a summary of her research at the following site;
http://www.natmus.dk/cons/reports/2001/ys_phd/pvcphd.htm
She states 'Degradation of objects was first detected within 10-35
years of acquisition.'
She also has an article 'Deterioration and conservation of plasticized
poly(vinyl chloride) objects' in the ICOM-CC 13th Triennial Meeting, Rio
de Janeiro, 22-27 September 2002: preprints. Unfortunately I don't have
a copy of that article.
Hope this is helpful
Joanne Hackett
V&A
>>> HadleyJ@xxxxxxxxxxxxx 03/07/2008 16:18 >>>
Hello all,
Do any of you have, or know where I can find information on the life
span of vinyl fabric? My colleagues have suggested will last 100 years,
but I thought it had more of a 10 year life span.
Thanks much!
Jennifer Hadley
Museum of Church History and Art
Registrar/Textile Conservator
801-240-0297
801-240-5342 (fax)
hadleyj@xxxxxxxxxxxxx
----------------------------------------------------------------------
NOTICE: This email message is for the sole use of the intended
recipient(s) and may contain confidential and privileged information.
Any unauthorized review, use, disclosure or distribution is prohibited.
If you are not the intended recipient, please contact the sender by
reply email and destroy all copies of the original message.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________
- --------------------------------------------------------------
China Design Now
Sponsored by HSBC
15 March - 13 July 2008 at V&A South Kensington
Book now on www.vam.ac.uk/chinadesignnow
A Century of Olympic Posters
17 May - 7 September 2008 at V&A Museum of Childhood
Admission free
Keep in touch - visit www.vam.ac.uk and sign up for our regular e-newsletter
- ---------------------------------------------------------------
The information contained in this message is confidential and intended only
for the individual named above. If you are not the intended recipient, or responsible for delivering it to the intended recipient you are hereby notified that any dissemination, distribution, copying, or disclosure of this information is prohibited and may be unlawful. If you have received this communication in error, please notify us by telephone on 020 7942 2353. This message has been scanned for viruses by the MessageLabs Email Security System.
______________________________________________________________________
----------------------------------------------------------------------
NOTICE: This email message is for the sole use of the intended recipient(s) and may contain confidential and privileged information. Any unauthorized review, use, disclosure or distribution is prohibited. If you are not the intended recipient, please contact the sender by reply email and destroy all copies of the original message.