I think rolling quilts for storage is usually best, especially if the quilt is very heavy.  I have seen old quilts with wool battings that have been folded and have been quite surprised at how deeply imprinted the folds are - whether paeeded or not.
 
Elizabeth Richards, PhD.
Professer Emerita
University of Alberta
 