Jennifer,

I recently obtained samples of naturally coloured cotton from Sally Fox's company Vreseis Limited (www.vreseis.com).  The cotton that they sell is organically grown and is the result of a breeding program  using stock originally used by the Cajun community in Lousiana. This naturally coloured cotton is not directly related to those used in ancient Peru (i.e. Gossypium barbadense).  You might try contacting Peru Naturtex Partners (www.perunaturtex.com). Their website provides a lot of information about naturally coloured Peruvian cottons.

Jan Vuori

Textile Conservator
Canadian Conservation Institute
1030 Innes Road
Ottawa, Ontario
Canada K1A 0M5
Tel: (613) 998-3721 ext. 275
Fax: (613) 998-4721
email: jan_vuori@xxxxxxxxx
www.cci-icc.gc.ca