I'll second the recommendations for the 21st Century Iron. I use mine quite a 
bit and it has held up well. (no handle problems in four + years- I must be 
lucky!).  One  other warning- the actual temperature of the iron is 
considerably less than that on the dial setting- I recommend measuring the 
temperature at the head and then adjusting the dial accordingly.

Nancy Pollak, Art Care Associates