Karen,

We have a long-standing brittle books program at the University of Maryland 
Libraries Preservation Department.  Our procedures are on the Web at 
http://www.lib.umd.edu/TSD/PRES/brittleunit.html
The process is managed with an Access database and our form is an Access 
report.  I will fax you copies of it.  We are fortunite to have a professional 
librarian, Susan Koutsky, to head that unit.  Sue's email address is 
sk197@xxxxxxxxxxxxxx  Please contact Sue for more specific information about 
the Access database if you like.

Yvonne


On Thu, 18 Oct 2001 13:22:33 -0400 Karen Brown <kebrown@xxxxxxxxxxxxxx> wrote:

> Dear PADG:  I would like to ask a favor of PADG subscribers.  I am in the 
> process of revising our selection form/process for brittle books and others 
> than cannot be reasonably repaired or rebound.  To assist this I would very 
> much like to attain copies of selection forms and/or procedures from as 
> many academic libraries as possible.  If you are willing to pull this on my 
> behalf and forward it to me, either electronically or through the postal 
> service, I would very much appreciate it.
> 
> Thank you in advance for your input.  Regards, Karen Brown/University at Albany
> Karen Brown
> Preservation Librarian
> University Libraries - LE 310
> University at Albany
> State University of New York
> 1400 Washington Ave.
> Albany, NY 12222
> 
> phone  518 437-3925
> fax  518 437-3930
> 

*******************************************************************
Yvonne Carignan                     Email:      yc38@xxxxxxxxxxxxx
Preservation Department Head        VoiceMail:  301-405-9343
McKeldin Library                    FAX:        301-341-9971
University of Maryland 
College Park, MD 20742





[Subject index] [Index for current month] [Table of Contents]