In a message dated 4/25/00 12:49:44 AM, jcollins@ccp.arizona.edu writes:

<< One of our artists has requested that we frame her prints using wood
spacers that sit directly on the edge of her art work. >>

If the purpose is to keep the glazing off the art, why not use FrameSpace or 
Econospace from FrameTek and seal the rabbet with acrylic tape (some of them 
have just been recommended on this forum).

Paul Frederick, CPF