[Table of Contents] [Search]


[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]

[frameconnews] Re: nicotine on bronze paint



Continuing the theme of nicotine on bronze paint on frame:

A bronze painted surface that has already been cleaned with soap and 
water may now be rid of its nicotine film.  Any remaining brown and 
dull material may be the oxidized surface of the bronze paint.

Hugh Glover

------------------------------------------------------------------------