Extra Extra Large Art: Conservation Treatment of the Garibaldi
Panorama at NEDCC

NEDCC's paper conservators recently worked on a project that could
be classified as extra extra large.  The Garibaldi Panorama is among
the longest paintings in the world, measuring 260 feet long and 41/2
feet high.  From the Anne S.K. Brown Military Collection at the John
Hay Library of Brown University, the two-sided work of art on paper
depicts the life story of Italian patriot Giuseppe Garibaldi, who
played a major role in the unification of Italy.

The Panorama was treated at NEDCC over a period of ten months, and
the painting, on a 16-foot table, became a familiar sight in the
paper conservation lab.

Learn more

    <URL:http://www.nedcc.org/about/nedcc-stories/garibaldi-panorama>

Northeast Document Conservation Center
Andover, MA


                                  ***
                  Conservation DistList Instance 27:45
                  Distributed: Saturday, May 17, 2014
                       Message Id: cdl-27-45-001
                                  ***
Received on Thursday, 15 May, 2014

[Search all CoOL documents]


Feedback for CoOL webmaster