Janet Berry <janet.berry [at] live__co__uk> writes

>Bubble Wrap--bubbles inside or outside? (With an intervention layer
>between the object and the Bubble Wrap.)

The age-old question.  The bubbles go on the outside to reduce
point-stress on the object surface and to avoid circular marks if
moisture gets trapped between the wrap and the object surface.  The
intervention layer will help avoid that problem so it's good to
include it.  Make sure that the wrap is polyethylene and doesn't
contain any PVC, which some of the cheaper wraps do.

Paul S. Storch
Project Specialist II/Collections Liaison
Historic Sites and Museums
B-124.2
Minnesota Historical Society
345 Kellogg Blvd. West
St. Paul, MN 55102-1906
651-259-3257
Fax: 651-297-2967


                                  ***
                  Conservation DistList Instance 24:30
                 Distributed: Sunday, December 19, 2010
                       Message Id: cdl-24-30-005
                                  ***
Received on Wednesday, 15 December, 2010

[Search all CoOL documents]


Feedback for CoOL webmaster