Conservation DistList Archives [Date] [Subject] [Author] [SEARCH]

Subject: Nitrate film

Nitrate film

From: Elizabeth Branigan <elizabeth.branigan<-at->
Date: Wednesday, August 25, 2010
I have had a query from a local library who have had a film returned
to them from the Film and TV Archive marked nitrate. They have asked
me for advice on how to dispose of it. So far they have received a
very expensive quote from a waste disposal firm. Neither the Fire
Brigade nor their local waste management site will touch it. Does
anyone have any suggestions?

Liz Branigan