Gulsu Simsek <simsekg [at] itu__edu__tr> writes

>I am looking for the Raman spectrum of Ag2S crystal. If someone
>works about the Raman characterization of corrosion products of
>silver, can he/she contact me?

You may want to try to contact someone in the analytical
laboratories at Eastman Kodak in Rochester, New York.