Subject: Incralac

Incralac

From: Mark Vine <vpackthread>
Date: Tuesday, August 29, 2006
George Bailey <george.bailey [at] awm__gov__au>

>For decades Incralac (made in Australia by Wattyl) has been the
>preferred coating for silver, copper and copper alloys at the
>Austalian War Memorial. Our preferred method of application is dip
>coating. Recently, however, Wattyl has ceased supplying Incralac in
>500 ml and 1 litre tins, and now only supplies it in aerosol cans.
>
>Can anyone recommend a viable alternative that is available in
>Australia?

For many years we have had a number of specialist metal cleaning,
protective metal coating, and metal lacquer products such as
Incralac and Frigilene manufactured for us in the United Kingdom.

We will continue to offer these and other conservation chemical
products in small amounts for use by conservators around the world.

Mark Vine
Conservation Resources (UK) Ltd
England


                                  ***
                  Conservation DistList Instance 20:12
                 Distributed: Friday, September 1, 2006
                       Message Id: cdl-20-12-003
                                  ***
Received on Tuesday, 29 August, 2006

[Search all CoOL documents]


URL: http://
Timestamp:
Retrieved: